Touch-up coatings for galvanizing damage

  • Touch-up

    Touch-up
    for damaged area

  • Bright Metallic Silver

  • AI Zn

    Al, zinc flake contained

Properties
  • Corrosion resistance
  • Improves performance by achieving high corrosion resistance even with a thin film of 3~5㎛. Suitable for restoring the performance of damaged parts such as scratches and blackening on galvanizing surfaces.
  • Workability
  • Spray the can with a light side-to-side swing to form a thin coat. It is a spray-on type that naturally cures at room temperature and dries quickly within 15 minutes.
  • Eco-friendly
  • When applying hot-dip galvanizing guardrail repair technology, carbon emissions are reduced by 99.4% compared to the production of new guardrails. It is a 'Safety Confirmed Household Chemical Product' that does not contain harmful substances such as xylene, toluene, and ethylbenzene.
Applications
Apply to
It can be applied to discolored, scratched galvanizing.
  • Scratched area

  • Discolored area

  • Same color as galvanizing after touchup

Related Solutions
Use Innotouch after G-SAVE for areas with severe corrosion.
Use G+PLUS after applying Innotouch for additional corrosion protection.